A single-phase full-color emitting phosphor Sr2Ca2La(PO4)3O∶Eu2+,Tb3+,Mn2+was synthesized by the high temperature solid-state method.The phase formation,luminescence properties,thermal stability,and energy transfer from Eu2+toTb3+and Eu2+to Mn2+in Sr2Ca2La(PO4)3O were investigated in details.Tunable emission color from blue to blueish green or orange can be observed under 365 nm near-ultraviolet excitation based on the energy transfer from Eu2+to Tb3+or Mn2+ions by varying the ra-tio of Eu2+/Tb3+or Eu2+/Mn2+ions.White light was obtained with chromaticity coordinates of(0.3558,0.3500)in the Sr2Ca2La(PO4)3O∶0.04Eu2+,0.08Tb3+,0.40Mn2+phosphor,suggesting their potential ap-plications in white light emitting diodes.