The electrochemical polymerization of methylene green has been carried out using cyclic voltammetry. The electrolytic so lution consisted of 4 × 10-3 mol/L methylene green, 0.1 mol/L NaNO3 and 1 × 10-2 mol/L sodium tetraborate with pH 11.0. The temperature for polymerization is controlled at 60℃. The scan potential is set between -0.2 and 1.2 V (vs. Ag/AgCl with saturated KCl solution). There are an anodic peak and a cathodic peak on the cyclic voltammogram of poly(methylene green) at pH≤3.8. Both peak potentials shift towards nega tive potentials with increasing pH value, and their peak cur rents decrease with increasing pH value. Poly(methylene green) has a good electrochemical activity and stability in aqueous solutions with pH ≤ 3.8. The UV-Visible spectrum and FTIR spectrum of poly (methylene green) are different from those of methylene green.