The effects of SrTiO3 on the hydrogen storage properties of MgH 2 have been studied for the first time. The onset dehydrogenation temperature of the MgH 2 -10 wt% SrTiO3 is found to be 275 ℃, which is 55 ℃ lower as compared to the as-milled MgH 2 . The composite is able to absorb 4.3 wt% of hydrogen in 60 min instead of 1.1 wt% for the as-milled MgH2 . Meanwhile, the composite is able to release 5.3 wt% of hydrogen in 17 min compared to 1.9 wt% by the as-milled MgH 2 at 320 ℃. The calculated E a of the MgH2 -10 wt% SrTiO3 is 109 kJ/mol, which is 26.3 kJ/mol lower than the calculated E a of the as-milled MgH2 . The SrTiO3 is not decomposed during the ball milling and the re/dehydrogenation processes. The catalytic effect shown by the SrTiO3 is owing to its ability to change the physical structure of the MgH2 particles during the ball milling process.